Abstract: Effective passivation of lithium metal surfaces, and prevention of battery-shorting lithium dendrite growth, are critical for implementing lithium-metal-anodes for batteries with increased power densities. Nanoscale surface heterogeneities can be "hot spots" where anode passivation breaks down. Motivated by the observation of lithium dendrites in pores and grain boundaries in all-solid batteries, we examine lithium metal surfaces covered with Li(2)O and/or LiF thin films with grain boundaries in them. Electronic structure calculations show that, at >0.25 V computed equilibrium overpotential, L(2)O grain boundaries with sufficiently large pores can accommodate Li(0) atoms which aid electron leakage and passivation breakdown. Strain often accompanies Li-insertion, applying a ~1.7% strain already lowers the computed overpotential to 0.1 V. Lithium metal nanostructures as thin as 12 Angstroms are thermodynamically favored inside cracks in Li(2)O films, becoming "incipient lithium filaments." LiF films are more resistant to lithium metal growth. The models used herein should in turn inform passivating strategies in all-solid-state batteries.

Summary

No one has generated a summary of this paper yet.

Paper to Video (Beta)

No one has generated a video about this paper yet.

Whiteboard

No one has generated a whiteboard explanation for this paper yet.

Open Problems

We haven't generated a list of open problems mentioned in this paper yet.

Continue Learning

We haven't generated follow-up questions for this paper yet.

Collections

Sign up for free to add this paper to one or more collections.