Universal Chemomechanical Design Rules for Solid-Ion Conductors to Prevent Dendrite Formation in Lithium Metal Batteries

Published 15 Jan 2019 in cond-mat.mtrl-sci | (1901.04910v1)

Abstract: Dendrite formation during electrodeposition while charging lithium metal batteries compromises their safety. While high shear modulus solid-ion conductors (SICs) have been prioritized to resolve pressure-driven instabilities that lead to dendrite propagation and cell shorting, it is unclear whether these or alternatives are needed to guide uniform lithium electrodeposition, which is intrinsically density-driven. Here, we show that SICs can be designed within a universal chemomechanical paradigm to access either pressure-driven dendrite-blocking or density-driven dendrite-suppressing properties, but not both. This dichotomy reflects the competing influence of the SICs mechanical properties and partial molar volume of Li+ relative to those of the lithium anode on plating outcomes. Within this paradigm, we explore SICs in a previously unrecognized dendrite-suppressing regime that are concomitantly soft, as is typical of polymer electrolytes, but feature atypically low Li+ partial molar volume, more reminiscent of hard ceramics. Li plating mediated by these SICs is uniform, as revealed using synchrotron hard x-ray microtomography. As a result, cell cycle-life is extended, even when assembled with thin Li anodes and high-voltage NMC-622 cathodes, where 20 percent of the Li inventory is reversibly cycled.

Summary

No one has generated a summary of this paper yet.

Paper to Video (Beta)

No one has generated a video about this paper yet.

Whiteboard

No one has generated a whiteboard explanation for this paper yet.

Open Problems

We haven't generated a list of open problems mentioned in this paper yet.

Continue Learning

We haven't generated follow-up questions for this paper yet.

Collections

Sign up for free to add this paper to one or more collections.